MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PP 9710 PP (Americas)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV stability. This material can exhibit ductility at temperatures as low as 0 degrees C. IMDS ID: 164207488

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Time 173000 sec
0.0050 in/in
@Time 48.0 hour
SABIC method
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Time 173000 sec
0.0090 in/in
@Time 48.0 hour
SABIC method
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 14.0 MPa2030 psi50 mm/min, 1A; ISO 527
Tensile Strength, Yield 20.0 MPa2900 psi50 mm/min; ISO 527
Elongation at Break 23.2 %23.2 %50 mm/min; ISO 527
Elongation at Yield 3.5 %3.5 %50 mm/min; ISO 527
Tensile Modulus 1.92 GPa278 ksi1mm/min; ISO 527
Flexural Modulus 2.02 GPa293 ksi2 mm/min, 64mm span; ISO 178
Izod Impact, Notched 0.180 J/cm0.337 ft-lb/in80*10*4mm, Cut; ISO 180/1A
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
80*10*4mm, Cut; ISO 180/1A
 6.00 kJ/m²
@Temperature 0.000 °C
2.86 ft-lb/in²
@Temperature 32.0 °F
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²80*10*4mm, Cut; ISO 179/1eA
 0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
 0.500 J/cm²
@Temperature 0.000 °C
2.38 ft-lb/in²
@Temperature 32.0 °F
80*10*4mm, Cut; ISO 179/1eA
Dart Drop, Total Energy 19.0 J14.0 ft-lbpeak, 23°C @ 6.6 m/s; ASTM D3763
 18.0 J
@Temperature 0.000 °C
13.3 ft-lb
@Temperature 32.0 °F
peak @ 6.6 m/s; ASTM D3763
 19.0 J
@Temperature -30.0 °C
14.0 ft-lb
@Temperature -22.0 °F
peak @ 6.6 m/s; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
@Temperature -30.0 - 100 °C
27.2 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
CTE, linear, Transverse to Flow 147 µm/m-°C
@Temperature -30.0 - 100 °C
81.7 µin/in-°F
@Temperature -22.0 - 212 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °F80*10*4mm, Cut; ISO 75-1&2
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C138 °F80*10*4mm, Cut; ISO 75-1&2
Vicat Softening Point 133 °C271 °F10N, 50°C/hr; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 210 - 270 °C410 - 518 °FInjection Molding
Zone 1 190 - 230 °C374 - 446 °F
Zone 2 200 - 250 °C392 - 482 °F
Zone 3 210 - 270 °C410 - 518 °F
Melt Temperature 210 - 270 °C410 - 518 °F
Mold Temperature 15.0 - 60.0 °C59.0 - 140 °F
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Back Pressure 1.00 - 1.50 MPa145 - 218 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11375 / 244842

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.