MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi FGF Recycled ABS-X 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; ABS Polymer

Material Notes: FGF Recycled ABS-X is a next-generation ABS. FGF recycled ABS-X is the perfect material for strong objects that require a high impact tolerance.

Features:

  • Enhanced mechanical properties over regular ABS
  • Great strength & aesthetics
  • Low warp
Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccISO 1183
Melt Flow 31 g/10 min
@Load 5.00 kg,
Temperature 200 °C
31 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 27.0 MPa3920 psiISO 527
Tensile Strength, Yield 42.0 MPa6090 psiISO 527
Elongation at Break 9.0 %9.0 %ISO 527
Elongation at Yield 3.0 %3.0 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
Charpy Impact, Notched 4.65 J/cm²22.1 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 76.0 °C169 °FISO 306 B
 
Processing PropertiesMetricEnglishComments
Zone 1 165 - 205 °C329 - 401 °F
Zone 2 180 - 220 °C356 - 428 °F
Zone 3 180 - 220 °C356 - 428 °F
Die Temperature 200 - 240 °C392 - 464 °F
Drying Temperature 75.0 °C167 °F<250 ppm
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Mass Temperature234°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9816 / 301041

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.