MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C70390, H10 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Spring

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 320
@Load 3.00 kg
320
@Load 6.62 lb
Tensile Strength 1000 MPa145000 psiTypical
 903 - 1100 MPa131000 - 160000 psi
Tensile Strength, Yield 862 - 1060 MPa125000 - 154000 psi0.2% Offset
 965 MPa140000 psi0.2% Offset, Typical
Elongation at Break 1.0 %1.0 %
Tensile Modulus 130 GPa18800 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000410 ohm-cm0.00000410 ohm-cm42% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 14.7 W/m-K102 BTU-in/hr-ft²-°F
Melting Point 1042 - 1095 °C1908 - 2003 °F
Solidus 1042 °C1908 °F
Liquidus 1095 °C2003 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 0.10 - 0.80 %0.10 - 0.80 %
Copper, Cu 91.7 - 97 %91.7 - 97 %As Balance
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg <= 0.20 %<= 0.20 %
Manganese, Mn <= 0.20 %<= 0.20 %
Nickel, Ni 2.3 - 4.6 %2.3 - 4.6 %
Silicon, Si 0.60 - 1.3 %0.60 - 1.3 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC70390x1 / 292444

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.