Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.- High dimensional stability
- High rigidity
- Excellent heat resistance for online-painting
- Mineral filled (9%)
Information provided by Styrolution |