MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC SABIC® PP 58MNK10 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This grade combines an excellent stiffnesswith high impact resistance. It has a low tendency to warp. Excellent flow in combination with high crystallisation speed enables outstanding processability aiming at easy mould filling and short cycle times. Thanks to the mentioned performance this grade is typically used in several kinds of containers. The excellent gloss level makes this material also favourable for household applications. This product is not intended for and must not be used in any pharmaceutical/medical applications. This grade material is UL registered under File E111275. IMDS 80775790

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-2 1A
Elongation at Yield 4.0 %4.0 %Speed of testing: 50 mm/min; ISO 527-2 1A
Tensile Modulus 1.55 GPa225 ksiSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²ISO 180/1A
 6.00 kJ/m²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 7.00 kJ/m²
@Temperature 0.000 °C
3.33 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 1.25 J/cm²5.95 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FFlat wise ( testbar 80*10*4mm); ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FFlat wise ( testbar 80*10*4mm); ISO 75
Vicat Softening Point 80.0 °C176 °Fat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 151 °C304 °Fat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentFalse
Nucleating agentTrue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11222 / 244689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.