MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain Tygon® SPT-3370 I.B. Sanitary Silicone Pressure Tubing Formulation
Categories: Polymer; Thermoset; Silicone

Material Notes: Tygon® 3370 I.B. : Often specified in high-purity applications, Tygon® Sanitary Silicone Pressure Tubing is produced from a platinum-curing process that helps ensure the highest level of biocompatibility available. The ultra smooth inner surface and the ability to be cleaned and sterilized repeatedly in CIP and SIP systems helps to maintain fluid integrity throughout sensitive fluid transfer or processing. When used in combination with sanitary fittings, complete assemblies can be constructed that provide the sanitary conditions critical to pharmaceutical, biotechnology, cosmetic, food, dairy and beverage applications. Braid-reinforced for increased pressure resistance, it also provides flexibility, durability, and chemical and temperature resistance to make it the ideal pressure tubing for a wide variety of industries.

Features/Benefits:
  • Consistently smooth inner surface limits particle entrapment
  • Platinum cured to minimize extractables
  • Tough braid reinforcement permits use under elevated working pressures
  • Withstands repeated CIP and SIP cleaning and sterilization
  • Ideal for use with Tygopure™ Reusable Sanitary Fittings
Typical applications include Sterile Filling, Media Dispensing, Vaccine Manufacturing, Bioreactor Process Lines, Water Purification Systems, Food and Dairy Processing, Diagnostic Test Product Manufacturing, Sanitary Fitting Assembly
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792-91
Water Absorption 0.11 %0.11 %24 hours at 23°C; ASTM D570-81
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 707015 seconds; ASTM D2240-91
Tensile Strength, Yield 8.27 MPa1200 psiASTM D412-92
Elongation at Break 500 %500 %ASTM D412-92
200% Modulus 4.48 MPa
@Strain 200 %
650 psi
@Strain 200 %
ASTM D412-92
Tear Strength 43.8 kN/m250 pliInitial Tear Strength; ASTM D624-91 Die B
Compression Set  3.0 %
@Temperature 70.0 °C
3.0 %
@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
 10 %
@Temperature 175 °C
10 %
@Temperature 347 °F
Constant Deflection, for 22 hrs.; ASTM D395-89
Tensile Set 25 %25 %ASTM D412-92
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.6 kV/mm600 kV/inASTM D149-93
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Brittleness Temperature -80.0 °C-112 °FASTM D746-79
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® LP 1500 Low Permeation Fuel Tubing
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Saint-Gobain Tygon® A-60-F Food Process Tubing Formulation

PSTGQZ194 / 68708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.