MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kraiburg TPE THERMOLAST® K TC7LEZ Thermoplastic Elastomer (UV/FG Series) Adhesion to PP
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The UV/FG series is a material solution for applications requiring UV resistance and adhesion to PP. The compounds are suitable for automotive exterior applications and available in black.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Black
Typical applications:
  • Roof racks
  • Static window encapsulations
  • Water deflectors
  • Bumpers
  • Cowls gaskets
  • Function and design elements
  • Automotive Exterior
  • Door sills
Material advantages:
  • Weather resistant, suitable for automotive exterior
  • Optimized flow properties
  • Surface mapping
  • Optimized mechanical properties
  • Adhesion to PP
  • In-process recycling possible
  • Temperature stability up to 100 °C

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³DIN EN ISO 1183-1
Spiral Flow 79.0 cm
@Pressure 76.0 MPa,
Temperature 200 °C
31.1 in
@Pressure 11000 psi,
Temperature 392 °F
DSOP Lab 2032
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070DIN ISO 48-4
Tensile Strength 10.0 MPa1450 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 700 %700 %200 mm/min; DIN 53504/ISO 37
Tear Strength 21.0 kN/m120 pliISO 34-1 Method B (b)
Compression Set  35 %
@Temperature 23.0 °C,
Time 259000 sec
35 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 47 %
@Temperature 70.0 °C,
Time 86400 sec
47 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 74 %
@Temperature 100 °C,
Time 86400 sec
74 %
@Temperature 212 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8331 / 308995

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.