MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Ecronova® KS 447 Styrene Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Ecronova® KS 447 is a styrene-acrylic emulsion that shows excellent adhesion on various metal substrates and very good corrosion protection results can be obtained. Because of the given elasticity the emulsion shows a good impact resistance. As well the emulsion shows a good water- and condensation resistance. Ecronova KS 447 is APEO free.

Markets: Paints and Coatings

Applications: Industrial Coatings, Metal Coatings

Related Products: BarrierPro 4545, Ecronova RA 576 H, Ecronova RA 127

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 49 - 51 %
pH 7.0 - 9.0
Viscosity 1000 - 4000 cP
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 27.0 °C
 
Descriptive Properties
Minimum Film Formation Temperature (°C)15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMCP9978 / 250453

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.