Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: - Designed for compression molding for optimal strength on large-span covers
- Excellent resistance to automotive chemicals and fluids, and to salt spray
- Replaces cast metals for reduced Noise, Vibration, and Harshness, plus molded-in color
- Excellent dimensional stability and creep resistance
- Excellent thermal properties and elevated temperature modulus retention
Market: Composite PowerTrain Information provided by Premix. A. Schulman has acquired this former Premix product line. |