MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik APM 2723 Hot Isostatic Pressed (HIP) Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: APM 2723 is a high alloyed powder metallurgical high speed steel corresponding to ASTM M3:2 with a combination of very good abrasive wear resistance and high compressive strength. Suitable areas of use include demanding cold-work applications like blanking of harder materials like carbon steel or cold-rolled strip steel, as well as use for cutting tools. As with all powder metallurgy tool steels, machinability and grindability are superior to conventional high speed steel due to the very fine microstructure. Thanks to the fully homogenous material achieved in the powder metallurgy process, the dimensional stability after heat treatment is excellent. The process also ensures that the cleanliness of the steel is very high with a low amount of non-metallic inclusions.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.98 g/cc0.288 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C  52
@Temperature 980 °C
52
@Temperature 1800 °F
tempering temperature 600°C
 55
@Temperature 1050 °C
55
@Temperature 1920 °F
tempering temperature 600°C
 57
@Temperature 1100 °C
57
@Temperature 2010 °F
tempering temperature 600°C
 58
@Temperature 980 °C
58
@Temperature 1800 °F
tempering temperature 560°C
 60
@Temperature 980 °C
60
@Temperature 1800 °F
tempering temperature 520°C
 60
@Temperature 1150 °C
60
@Temperature 2100 °F
tempering temperature 600°C
 60
@Temperature 1050 °C
60
@Temperature 1920 °F
tempering temperature 560°C
 62
@Temperature 1050 °C
62
@Temperature 1920 °F
tempering temperature 520°C
 62
@Temperature 1180 °C
62
@Temperature 2160 °F
tempering temperature 600°C
 62.5
@Temperature 1100 °C
62.5
@Temperature 2010 °F
tempering temperature 560°C
 64
@Temperature 1100 °C
64
@Temperature 2010 °F
tempering temperature 520°C
 64.5
@Temperature 1150 °C
64.5
@Temperature 2100 °F
tempering temperature 560°C
 66
@Temperature 1180 °C
66
@Temperature 2160 °F
tempering temperature 560°C
 66
@Temperature 1150 °C
66
@Temperature 2100 °F
tempering temperature 520°C
 66.5
@Temperature 1180 °C
66.5
@Temperature 2160 °F
tempering temperature 520°C
Modulus of Elasticity 230 GPa33400 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 µm/m-°C
@Temperature 20.0 - 100 °C
6.00 µin/in-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.23 %1.23 %
Chromium, Cr 4.2 %4.2 %
Molybdenum, Mo 5.0 %5.0 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 3.1 %3.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Kanthal APMT Seamless tube and pipe
Sandvik Osprey 1.2709 Tool Steel Powder
Sandvik Osprey 18Ni300 Tool Steel Powder
Sandvik Osprey A6 Tool Steel Powder
Sandvik Kanthal SW 100 Spray Wire

NSANDV5280 / 199844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.