MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Covestro DESMODUR® MLQ22165 + BAYTEC® L20 + BAYTEC® XL B (Catalyst SD11-2) 80 A Polyurethane, MDI- Caprolactone
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccBAYTEC® XL B
 1.04 g/cc1.04 g/ccBAYTEC® L20
 1.13 g/cc1.13 g/ccDESMODUR® MLQ22165
 1.15 g/cc1.15 g/cc
Viscosity 30 cP30 cPBAYTEC® XL B
 300 cP300 cPBAYTEC® L20
 560 cP560 cPDESMODUR® MLQ22165
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080DIN 53505
 78
@Temperature 80.0 °C
78
@Temperature 176 °F
DIN 53505
 84
@Temperature -5.00 °C
84
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 50.0 MPa7250 psiDIN 53504
Tensile Stress at Strain 1.90 MPa
@Strain 10 %
276 psi
@Strain 10 %
DIN 53504
Elongation at Break 520 %520 %DIN 53504
100% Modulus 5.30 MPa
@Strain 100 %
769 psi
@Strain 100 %
DIN 53504
200% Modulus 8.10 MPa
@Strain 200 %
1170 psi
@Strain 200 %
DIN 53504
300% Modulus 12.3 MPa
@Strain 300 %
1780 psi
@Strain 300 %
DIN 53504
Resilience 6363[%]; DIN 53512
Tear Strength 39.1 kN/m223 pliwith nick; ISO 34-1
 89.1 kN/m508 pliwithout nick; ISO 34-1
Abrasion 2020[mm3]; ISO 4649
Compression Set 25 %
@Temperature 70.0 °C,
Time 79200 sec
25 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FDESMODUR® MLQ22165
 45.0 °C113 °FBAYTEC® XL B
 70.0 °C158 °FBAYTEC® L20
Mold Temperature 100 °C212 °F
Pot Life 7.50 min7.50 min
 
Descriptive Properties
AppearancesolidDESMODUR® MLQ22165
 solidBAYTEC® L20
 solidBAYTEC® XL B
Content0.18SD11-2 catalyst % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 100Parts by weight of BAYTEC® L20
 12.8Parts by weight of BAYTEC® XL B
 16.3-16.7%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Covestro MONDUR® TD 80 Grade B Polyurethane
Covestro MONDUR® TD 80 Grade A Polyurethane
Covestro DESMODUR® MGQ32135 + BAYTEC® D13 + BAYTEC® XL B (Catalyst SD6-40 or SD6-160), 80 A Polyurethane, MDI-PPG

PCOVEST0496 / 202279

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.