MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Garlock 19 SBR Rubber Gasketing, Cotton Reinforced
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: SBR rubber with cotton sheeting as fabric insert

Combines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any service condition

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8575 - 85
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.22 kV/mm
@Thickness 3.17 mm
31.0 kV/in
@Thickness 0.125 in
Unconditioned; ASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.3 °C
@Pressure 1.72 MPa
200 °F
@Pressure 250 psi
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Z800 Commercial SBR Rubber
Garlock 60 SBR Sheet Rubber
ATG s.r.l. SBR Styrene-Butadiene Rubber
Garlock 2102 C.I. SBR/NBR Sheet Rubber, Polyester Insert
Garlock 50 Natural/SBR Sheet Rubber

PGARL850 / 157537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.