MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant Black Polyamide 6 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Clariant polyamide 6 3D printer filament is made of a good flowing Polyamide 6 that results in high performance 3D printed parts. Clariant Hostanox® P-EPQ® and Nylostab® S-EED® are added via a Renol® masterbatch to improve resistance to thermo-oxidative degradation and minimize yellowing due to ultraviolet radiation

General properties:

  • Semi-crystalline thermoplastic
  • High impact strength
  • High stiffness
  • Outstanding wear resistance
  • Good coefficient of friction
  • Very good temperature resistance

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.141 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 78.0 MPa50 mm/min, Injection Molded; ISO 527
Elongation at Break 20 %50 mm/min, Injection Molded; ISO 527
Flexural Strength 101 MPaInjection Molded; ISO 178
Flexural Modulus 2.48 GPaInjection Molded; ISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °CDSC 10°C/min (Natural Color); ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 165 °CInjection Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °CInjection Molded; ISO 75
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 - 280 °CPrint Temperature
 
Descriptive Properties
Printing Bed AdhesionDirectly on glass or polyimide film
 PEI surfacewith thin coat of PVP adhesive
Printing Bed Temperature70°C Ideal
Printing Fan SettingMedium to High
Printing Speed20 - 50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin
Clariant Black Polycarbonate 3D Printer Filament
Clariant Polyamide 12 3D Printer Filament
A. Schulman CP851 High Flow, Injection Molding Grade
Chevron Phillips Marlex® 7109DL LLDPE Blown Film Resin

PCLAR00004 / 230596

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.