MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical HIPS MI770 PS, Impact Modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: Injection Molding, PS, Impact Modified, High Gloss

Application: Electric/Electronic Components, Stationary Articles, Food Containers, etc.

CAS: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 6.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238 (G)
 16 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238 (I)
 69 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238 (G)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ASTM D785
Tensile Strength, Yield 350 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 79 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Yield 4.0 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Tensile Modulus 23000 kg(f)/cm²
@Thickness 3.20 mm
1mm/min; ASTM D638
Flexural Yield Strength 550 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Flexural Modulus 27200 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 5.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 6.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 11.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Strength 40.0 kV/mm
Arc Resistance 120 - 180 secASTM D495
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
Flammability, UL94 HB
@Thickness >=1.60 mm
 HB
@Thickness >=3.20 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 170 - 190 °CInjection Molding
Middle Barrel Temperature 180 - 200 °CInjection Molding
Front Barrel Temperature 190 - 210 °CInjection Molding
Nozzle Temperature 190 - 220 °CInjection Molding
Melt Temperature 190 - 220 °CInjection Molding
Mold Temperature 40.0 - 70.0 °CInjection Molding
Drying Temperature 80.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical ALPHALAC SG970 HIPS
LG Chemical ALPHALAC SG970NSU HIPS
LG Chemical HIPS 403AF PS, Flame Retardant
LG Chemical HIPS MI750 PS, Impact Modified
LG Chemical HIPS 60HRI PS, Impact Modified

PLAY612 / 148622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.