MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

308 Stainless steel, cold drawn wire, 50% hardened
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: UNS S30800, ASTM A167, ASTM A276, ASTM A314, ASTM A473, ASTM A580, SAE J405 (30308), DIN 1.4303, UNI X 8 CrNi 19 10, JIS SUS 305, JIS SUS 305 J1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 297
@Diameter 3.20 - 9.53 mm
297
@Diameter 0.126 - 0.375 in
Converted from Rockwell C hardness.
Hardness, Knoop 318
@Diameter 3.20 - 9.53 mm
318
@Diameter 0.126 - 0.375 in
Converted from Rockwell C hardness.
Hardness, Rockwell C 29 - 32
@Diameter 3.20 - 9.53 mm
29 - 32
@Diameter 0.126 - 0.375 in
Hardness, Vickers 308
@Diameter 3.20 - 9.53 mm
308
@Diameter 0.126 - 0.375 in
Converted from Rockwell C hardness.
Tensile Strength, Ultimate  895 - 1035 MPa
@Diameter 3.20 - 9.53 mm
130000 - 150100 psi
@Diameter 0.126 - 0.375 in
 895 - 1105 MPa
@Diameter 0.530 - 3.18 mm
130000 - 160300 psi
@Diameter 0.0209 - 0.125 in
 1140 - 1380 MPa
@Diameter 0.0510 - 0.510 mm
165000 - 200000 psi
@Diameter 0.00201 - 0.0201 in
Tensile Strength, Yield  725 - 860 MPa
@Diameter 3.20 - 9.53 mm
105000 - 125000 psi
@Diameter 0.126 - 0.375 in
 760 - 1035 MPa
@Diameter 0.530 - 3.18 mm
110000 - 150100 psi
@Diameter 0.0209 - 0.125 in
 895 - 1105 MPa
@Diameter 0.0510 - 0.510 mm
130000 - 160300 psi
@Diameter 0.00201 - 0.0201 in
Elongation at Break  11 - 18 %
@Diameter 0.0510 - 0.510 mm
11 - 18 %
@Diameter 0.00201 - 0.0201 in
in 50 mm
 11 - 18 %
@Diameter 0.530 - 3.18 mm
11 - 18 %
@Diameter 0.0209 - 0.125 in
in 50 mm
 11 - 18 %
@Diameter 3.20 - 9.53 mm
11 - 18 %
@Diameter 0.126 - 0.375 in
in 50 mm
Tensile Modulus 195 GPa28300 ksi
Izod Impact 135 - 165 J99.6 - 122 ft-lb
Charpy Impact >= 135 J>= 99.6 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000720 ohm-cm
@Temperature 20.0 °C
0.0000720 ohm-cm
@Temperature 68.0 °F
 0.000116 ohm-cm
@Temperature 650 °C
0.000116 ohm-cm
@Temperature 1200 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
9.89 µin/in-°F
@Temperature 32.0 - 599 °F
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  15.2 W/m-K
@Temperature 0.000 - 100 °C
105 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
 21.6 W/m-K
@Temperature 500 °C
150 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
Maximum Service Temperature, Air 925 °C1700 °FIntermittent
 980 °C1800 °FContinuous Service
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 20 %20 %
Iron, Fe 66 %66 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 11 %11 %
Phosphorus, P <= 0.045 %<= 0.045 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
308 Stainless steel, cold drawn wire, 25% hardened
308 Stainless steel, cold drawn wire, 75% hardened
308 Stainless steel, annealed, plate
308 Stainless steel, cold drawn wire, full hardened
347 Stainless Steel, cold drawn wire, 25% hard, 0.05-0.51 mm diameter

MQ308J / 12699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.