Description: TIPELIN BS 520-14 is a high density polyethylene copolymer (with hexen-1 as comonomer) grade for blow molding of products, which require very high ESCR and chemical resistance. The grade contains antioxidants and acid scavenger. Applications: TIPELIN BS 520-14 is recommended for hollowed products of maximum 220 liters capacity for aggressive industrial chemicals and surface active substances, thermoforming of extruded sheets. (1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). Information provided by Molgroup Chemicals |