MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® PC PC5800 PC (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC5800 resin is a very high flow (MFR = 8.9 at 250C/1.2kg) polycarbonate product designed for use in the optical media market. It is available exclusively at www.sabicpc.com.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Water Absorption 0.35 %23°C/sat; ISO 62
Moisture Absorption at Equilibrium 0.35 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 8.0 g/10 min
@Load 1.20 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 8.9 g/10 min
@Load 1.20 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
 60.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 40 %50mm/min; ISO 527
 >= 40 %50mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1mm/min; ISO 527
 2350 MPa50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 90.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.010
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Thermal Conductivity 0.200 W/m-KISO 8302
 0.200 W/m-KASTM C177
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 132 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 132 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 122 °C
@Thickness 3.20 mm
ASTM D648
Vicat Softening Point 138 °CRate B/50; ISO 306
 138 °CRate B/50; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
 1.586ISO 489
Haze <= 0.70 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible >= 90 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 340 - 370 °CInjection Molding
Zone 1 270 - 290 °C
Zone 2 320 - 340 °C
Zone 3 350 - 380 °C
Melt Temperature 340 - 370 °C
Mold Temperature 75.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10740 / 244207

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.