MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

American Alaska Cedar (Yellow Cedar) Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Conifer

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Chamaecyparis nootkatensis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1800 N405 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2300 N517 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 1.79 MPa260 psiPerpendicular to Grain*
Modulus of Rupture 0.0427 GPa6.20 ksiStatic Bending*
Flexural Yield Strength 24.8 MPa3600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 6.62 GPa960 ksiStatic Bending*
Compressive Strength 2.83 MPa410 psiPerpendicular to Grain*
 16.5 MPa2390 psiParallel to Grain*
 19.9 MPa2880 psiMax Crushing Strength Parallel to Grain*
Shear Strength 5.65 MPa820 psiParallel to Grain*
Impact 3.23.2in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 86008600psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00531 J/cm³0.770 in-lb/in³Static Bending*
Work to Maximum Load 0.0655 J/cm³9.50 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.108 W/m-K0.750 BTU-in/hr-ft²-°FOven Dry
 0.130 W/m-K0.900 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 2.8 %2.8 %Radial, from green to oven dry
 6.0 %6.0 %Tangential, from green to oven dry
 9.2 %9.2 %Volumetric, from green to oven dry

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Northern White Cedar (Eastern Arborvitae) Wood
1045 Aluminum Composition Spec
American Pine Wood
American Cedar Wood
American Eastern Red Cedar Wood

PTSA500 / 71257

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.