MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Apcotex Apcotex PC 200 Carboxylated Styrene Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Description: Apcotex PC 200 is a Carboxylated Styrene-Butadiene Latex used as a binder for metalized paper coating and Non-Woven Carpets. It is manufactured by employing state-of-the-art emulsion polymerization technology ensuring product consistency.

Advantages:

  • Provides good binding strength
  • Excellent metalized gloss
  • Easy to use in Non-Woven Carpets
  • No undesirable odor in the finished carpet
  • Excellent compatibility with fillers like Calcium Carbonate, China Clay and co binders like Carboxy Methyl Cellulose (CMC), Synthetic Acrylic thickener

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 49 - 51 %
pH 8.5 - 9.5
Brookfield Viscosity <= 300 cPLVF, SP.1, 12 RPM
Surface Tension 36 - 42 dynes/cm
Storage Temperature 5.00 - 40.0 °C
 
Descriptive Properties
AppearanceMilky white pourable liquid
Emulsifying SystemSynthetic anionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPCOT040 / 315619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.