MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman C-11 Ketone Solvent
Categories: Fluid; Solvent

Material Notes: Product Description: Eastman™ C-11 Ketone is a low-cost, slow-evaporating, low-density mixture of ketone solvents. It is useful as a retarder solvent for primers, coil coatings, maintenance coatings and high-solids enamels. In these coatings, C-11 Ketone improves gloss and leveling, reduces orange peel, minimizes solvent popping, and helps reduce the VOC content. In many coatings, it can be used alone or blended with other solvents to replace isophorone and dibasic esters. Eastman™ C-11 Ketone has good solvency for a wide range of resins including nitrocellulose, alkyds, polyesters, acrylics, epoxies, and some vinyl chloride/vinyl acetate copolymers. Compared with other solvents in the same evaporation range, Eastman™ C-11 Ketone often offers an economic advantage.

Application/Uses:

  • Coatings - Automotive OEM
  • Coatings - Automotive Refinish
  • Coatings - Can and Coil
  • Coatings - General Industrial
  • Coatings - Industrial Maintenance and Marine
  • Coatings - Industrial Wood
  • Coatings - Misc. (Thinners and Purge Solvents)
  • Coatings - Transportation
Key Attributes:
  • Good solvent activity
  • Low density
  • Low surface tension
  • Low water miscibility
  • Non-HAP
  • Non-SARA
  • REACH compliant
  • Readily biodegradable*
  • Slow evaporation rate

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.840 g/cc
Viscosity 2.1 cPLiquid
Vapor Pressure <= 0.00167 atm
Surface Tension 27.5 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.10
 
Thermal PropertiesOriginal ValueComments
CTE, linear 99.0 µm/m-°C
Melting Point -12.0 °CFreezing Point
Boiling Point 200 °C@ 760 mm Hg, Initial
 240 °C@ 760 mm Hg, Dry Point
Flash Point 84.0 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.435
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5210 / 222404

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.