MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

H.C. Starck Amperit® 119.075 Molybdenum-Nickel SF RC 60 75-25 (Mo / NiSF)
Categories: Metal; Nonferrous Metal

Material Notes: Composition is of NiSF RC 60 only

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 2.20 - 2.90 g/cc0.0795 - 0.105 lb/in³Mo; ASTM B212
 3.80 - 4.60 g/cc0.137 - 0.166 lb/in³NiSF RC 60; ASTM B212
Particle Size 20 µm20 µmMaximum of 3% less than, (NiSF RC 60)
 45 µm45 µmMaximum of 30% less than, (Mo)
 45 µm45 µmMaximum of 30%, Mo
 53 µm53 µmMaximum of 10% greater than, (NiSF RC 60)
 90 µm90 µmMaximum of 5% greater than, (Mo)
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.0 - 3.9 %3.0 - 3.9 %
Carbon, C 0.60 - 1.2 %0.60 - 1.2 %
Chromium, Cr 13 - 17 %13 - 17 %
Iron, Fe 2.4 - 4.6 %2.4 - 4.6 %
Nickel, Ni 68.4 - 77.1 %68.4 - 77.1 %
Silicon, Si 3.9 - 4.9 %3.9 - 4.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 335.066 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi)
Special Metals Nickel 200
Cast Stainless Steel 440C, EN 1088-3
H.C. Starck Amperit® 250.1 Water Atomized (NiCr 80-20)
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel

NHCSTA030 / 17232

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.