MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Denka Polymar Alloy HS-G193 PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Highly functional resin made by mixing ABS resins and polycarbonate resins. Good Flow. Uses: Exterior parts of automobiles.

Information provided by Denka Company Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
 1.13 g/cc0.0408 lb/in³ASTM D-792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 2.00 mm
0.0050 - 0.0070 in/in
@Thickness 0.0787 in
DENKA Method
Melt Flow 10 g/10 min
@Load 9.99 kg,
Temperature 220 °C
10 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D-785
 121121ISO 2039-2
Tensile Strength at Break 48.0 MPa6960 psi50 mm/min; ISO 527-1,-2
 56.0 MPa8120 psi5 mm/min; ASTM D-638
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ISO 527-1,-2
Tensile Modulus 2.46 GPa357 ksi1 mm/min; ISO 527-1, -2
Flexural Strength 88.0 MPa12800 psi15 mm/min; ASTM D-790
 93.0 MPa13500 psi2 mm/min; ISO 178
Flexural Modulus 2.55 GPa370 ksi2 mm/min; ISO 178
 2.55 GPa370 ksi15 mm/min; ASTM D-790
Izod Impact, Notched 6.37 J/cm11.9 ft-lb/inISO 179
Charpy Impact, Notched 7.50 J/cm²35.7 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C210 °FFlatwise; ISO 75-1, -2
 105 °C221 °FEdgewise; ASTM D-648
Vicat Softening Point  115 °C
@Load 5.10 kg
239 °F
@Load 11.2 lb
ISO 306
 115 °C
@Load 5.10 kg
239 °F
@Load 11.2 lb
ASTM D-1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 220 - 240 °C428 - 464 °FCylinder 1
 230 - 250 °C446 - 482 °FCylinder 2
 240 - 260 °C464 - 500 °FCylinder 3
Nozzle Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °Factual temperature of mold surface
Drying Temperature 110 °C
@Time 10800 - 18000 sec
230 °F
@Time 3.00 - 5.00 hour
Back Pressure 0.0345 - 0.103 MPa5.00 - 15.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDENJ840 / 250175

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.