MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexPly® 200/38%/644 Phenolic Resin, E glass, 8H satin
Categories: Polymer; Thermoset; Phenolic

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 380 MPa55100 psiWeft; pr EN2561
 520 MPa75400 psiWarp; pr EN2561
Flexural Strength 340 MPa49300 psiWeft; pr EN2562
 490 MPa71100 psiWarp; pr EN2562
Flexural Modulus 23.0 GPa3340 ksiWeft; pr EN2562
 29.0 GPa4210 ksiWarp; pr EN2562
Compressive Strength 365 MPa52900 psiWarp; DIN 65380
Shear Strength 40.0 MPa5800 psiInterlaminar, Warp; pr EN2563
 21.0 MPa
@Temperature 80.0 °C
3050 psi
@Temperature 176 °F
Interlaminar, Warp; pr EN2563
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 90.0 min
@Temperature 135 °C
1.50 hour
@Temperature 275 °F
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Fabric Weight305 g/m2E glass, 8H satin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9182 / 322338

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.