MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Blood Plasma
Categories: Fluid; Wood and Natural Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.022 - 1.026 g/cc
pH 7.39 - 7.45
Viscosity Measurement 1.18 - 1.59Relative Viscosity
Surface Tension 56.2 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8130 - 8547 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 3.93 J/g-°C
Melting Point -0.568 - -0.512 °CFreezing pt. Depression
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3485 - 1.3513
 
Descriptive Properties
Osmolality, mosm/kg279-295

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Whole Blood
Human Brain Matter
Human Femoral Artery
Human Iliac Artery
Human Carotid Artery

PTSXBI67 / 71553

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.