MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Film

Material Notes: Data provided by DuPont Packaging Polymers.

A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall toughness and gas permeability. Provides excellent qualities to the converter which make it an ideal film for printing and laminating. Its barrier properties and stiffness make it an excellent choice for a variety of packaging end uses such as snacks, processed meat, cheese, condiments.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/cc
Moisture Vapor Transmission 2.18 cc-mm/m²-24hr-atmASTM E398-70
Water Vapor Transmission 145 g/m²/dayASTM E398-70
Oxygen Transmission 0.590 cc-mm/m²-24hr-atmor 39 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66
Thickness 15.0 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 50 %ASTM D882
Film Elongation at Break, TD 250 %ASTM D882
Secant Modulus, MD 2.26 GPaASTM D882
Secant Modulus, TD 2.26 GPaASTM D882
Elmendorf Tear Strength, MD 3.00 g/micronASTM D1922-67
Elmendorf Tear Strength, TD 5.00 g/micronASTM D1922-67
Film Tensile Strength at Break, MD 240 MPaASTM D882
Film Tensile Strength at Break, TD 17.0 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %
Gloss 150 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness
Overview of materials for PEN-PET
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness
DuPont™ Dartek® N-201 Nylon 6,6 Non-Forming Film, 25 µm Thickness
DuPont™ Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness

PDU742 / 33161

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.