MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dynasol Solprene® 4321 Thermoplastic Rubber (SBS)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Solprene 4321 is a linear block copolymer of styrene and butadiene, with 32% styrene content, most of it forming polystyrene block, which gives the polymer a thermoplastic behavior. It has a non-staining antioxidant and also available version TNPP-BHT free antioxidant system; FDA approved for use in food contact applications and is essentially gel free with a very clear color. It is presented as free flowing porous crumb making easy its handling and dissolution

Uses: Solprene 4321 is used as compounding ingredient for adhesives. The product is an excellent modifier for asphalt applications including self adhesive roofing membrane and sealants. Also is used in thermoplastic injected shoe soles formulations.

Main Applications:
Roofing
Footwear
Polymer Modification
Adhesives

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Viscosity Measure 6.0 cSt6.0 cSt5.23% Toluene solution; NM-300-11
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
11 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Chemical PropertiesMetricEnglishComments
Styrene Content 31 %31 %Block; NM 202-07
 32 %32 %on polymer; ASTM D5775
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171ASTM D2240
Tensile Strength 3.50 MPa508 psiASTM D412
Elongation at Break 1250 %1250 %ASTM D412
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS)
Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS)
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)

PDYNA990 / 132985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.