MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow DX5E66 Polypropylene Homopolymer Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes:
    Overview
  • Consistent processability
  • Very high cleanliness
  • Good optical properties
  • Complies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No Objection

DX5E66 Developmental Polypropylene Resin is intended for use in cast film processes.

Braskem acquired Dow's polypropylene business. This specific grade was discontinued priot to the acquisition and so is listed as a discontinued Dow product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Thickness 50.8 microns2.00 milFilm Thickness
Melt Index of Compound 8.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.7 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Film Tensile Strength at Yield, MD 21.6 MPa3130 psiASTM D882
Film Tensile Strength at Yield, TD 15.7 MPa2280 psiASTM D882
Tensile Strength, Yield 33.0 MPa4790 psiASTM D638
Film Elongation at Break, MD 690 %690 %ASTM D882
Film Elongation at Break, TD 750 %750 %ASTM D882
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Modulus, 1% Secant 1380 MPa200000 psiASTM D790A
Secant Modulus, MD 0.719 GPa104 ksi2% secant modulus; ASTM D882
Secant Modulus, TD 0.693 GPa101 ksi2% secant modulus; ASTM D882
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256A
Elmendorf Tear Strength MD 64 g64 gASTM D1922
Elmendorf Tear Strength TD 88 g88 gASTM D1922
Dart Drop Test <= 100 g<= 0.221 lbFilm; 50.8 microns; ASTM D1709B
 110 g0.243 lbFilm; 50.8 microns; ASTM D1709A
Film Tensile Strength at Break, MD 50.3 MPa7300 psiASTM D882
Film Tensile Strength at Break, TD 45.1 MPa6540 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 161 °C322 °FDSC; Dow Method
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °FUnannealed; ASTM D648
Vicat Softening Point 155 °C311 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.22 %
@Thickness 0.0508 mm
0.22 %
@Thickness 0.00200 in
ASTM D1003
Gloss 95 %95 %ASTM D2457, 45°, 50.8 microns
 145 %145 %ASTM D2457, 20°, 50.8 microns
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Film Puncture Resistance (J/cm3)9.76Dow Method; 50.8 microns
Film Toughness (J/cm3)344TD: 50.8 microns; ASTM D882
 353MD: 50.8 microns; ASTM D882

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0437T20L Talc Reinforced
Braskem CP 401 HC Injection Molding Polypropylene
Braskem H 103 Injection Molding Polypropylene
Dow H700-12 Polypropylene Homopolymer Resin
LyondellBasell Adstif HA 3105 Polypropylene

PDOW0971 / 93307

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.