MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lotte Advanced Materials EPP-B11P Expanded Polypropylene Bead
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Foamed

Material Notes: EPP-B11P is a expanded polypropylene bead product. This grade is suitable for producing parts require high-compressive strength and impact resistance. the product has greater properties than any other foam products.

Applications: Automotive parts, packaging

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0820 g/cc0.00296 lb/in³ISO 845
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1.20 MPa174 psiISO 1798
Elongation at Break 19.0 %19.0 %ISO 1798
Compressive Strength 0.500 MPa72.5 psiISO 3386-1
Compression Set 7.00 %7.00 %ISO-1856-C
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0610 W/m-K0.423 BTU-in/hr-ft²-°FISO 8301
Flame Spread <= 100 mm/min<= 3.94 in/minFMVSS 302
Shrinkage 0.0190 %0.0190 %
 
Descriptive Properties
Odor>3MS 300-34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9090 / 325572

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.