MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® A3HG7 BK00565 Nylon 66, 35% Glass Fiber Reinforced (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Ultramid A3HG7 BK00565 is a 35% glass fiber reinforced, pigmented black injection molding PA66 grade.

Applications: Typical applications include machinery components and housings of high stiffness and dimensional stability such as gears, solenoid valve housings, electrical flow heaters, trailing cable attachments, as well as electrically insulating parts.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Melt Flow 29 g/10 min
@Load 5.00 kg,
Temperature 235 °C
29 g/10 min
@Load 11.0 lb,
Temperature 455 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 193 MPa28000 psiISO 527
Elongation at Break 2.8 %2.8 %ISO 527
Tensile Modulus 11.3 GPa1640 ksiISO 527
Flexural Strength 287 MPa41600 psiISO 178
Flexural Modulus 10.5 GPa1520 ksiISO 178
Izod Impact, Notched (ISO)  9.50 kJ/m²
@Temperature -40.0 °C
4.52 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 12.0 kJ/m²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  6.10 J/cm²
@Temperature -30.0 °C
29.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 7.70 J/cm²
@Temperature 23.0 °C
36.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.950 J/cm²
@Temperature -40.0 °C
4.52 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 263 °C505 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 253 °C487 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 45.0 - 105 °C113 - 221 °Fcan be used where applicable
 80.0 - 90.0 °C176 - 194 °Frecommended
 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8944 / 254902

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.