Description: The ALPA KAT series promote a quick, low temperature curing of the hydrosilylation reaction. The catalysts are available as solution in vinyl terminated polydimethylsiloxane (SFA 42 series) in different concentrations. They form silicone elastomers through an addition curing crosslinking reaction between Si-vinyl and Si-H groups. Key Features - Containing Karstedts's catalyst
- 1% Platinum
- Excellent reactivity
- No shrinkage during crosslinking
Key Applications- Catalyst for addition curing formulations
Information provided by CHT Group |