MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

SABIC LNP™ COLORCOMP™ Compound W1000PRB Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP COLORCOMP W1000PRB compound is based on Polybutylene Terephthalate (PBT) resin. Added features of this grade include: Healthcare, Food Contact Compliant, Biocompatible (ISO 10993 or USP Class VI), EtO and Gamma Sterilizable, Mold Release.

Features: Low Extractable,Aesthetics and Appearance,Healthcare,Steam, Gamma, EtO and E-beam sterilizable,Custom Color,Good Mold Release,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0800 %0.0800 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62-1
Viscosity 70 cP
@Load 2.16 kg,
Temperature 265 °C
70 cP
@Load 4.76 lb,
Temperature 509 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
@Thickness 3.20 mm
0.015 - 0.020 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 265 °C
80 g/10 min
@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.0 MPa3770 psi50 mm/min; ASTM D638
 49.0 MPa7110 psi50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ISO 527
 60.0 MPa8700 psi50 mm/min; ASTM D638
Elongation at Break 10 %10 %50 mm/min; ASTM D638
 10 %10 %50 mm/min; ISO 527
Elongation at Yield 3.2 %3.2 %50 mm/min; ISO 527
 3.7 %3.7 %50 mm/min; ASTM D638
Tensile Modulus 2.60 GPa377 ksi1 mm/min; ISO 527
 2.70 GPa392 ksi5 mm/min; ASTM D638
Flexural Strength 80.0 MPa11600 psi2 mm/min; ISO 178
 89.0 MPa12900 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.26 GPa328 ksi2 mm/min; ISO 178
 2.50 GPa363 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 30.0 J22.1 ft-lbASTM D256
 30.0 J
@Temperature -30.0 °C
22.1 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²80*10*4; ISO 180/1A
 2.00 kJ/m²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 20.0 J14.8 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
@Thickness 3.20 mm
302 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C120 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 54.0 °C
@Thickness 3.20 mm
129 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 180 °C356 °FRate B/50; ASTM D1525
 180 °C356 °FRate B/120; ISO 306
 183 °C361 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 25.0 - 35.0 °C77.0 - 95.0 °FWater Bath Temperature
Nozzle Temperature 240 - 255 °C464 - 491 °F
Zone 1 200 - 230 °C392 - 446 °FCompounding Extrusion
Zone 2 240 - 255 °C464 - 491 °F
 240 - 255 °C464 - 491 °FCompounding Extrusion
Zone 3 245 - 260 °C473 - 500 °F
 240 - 275 °C464 - 527 °FCompounding Extrusion
Zone 4 240 - 275 °C464 - 527 °FCompounding Extrusion
Adapter Temperature 240 - 275 °C464 - 527 °FCompounding Extrusion
Die Temperature 240 - 275 °C464 - 527 °FCompounding Extrusion
Melt Temperature 245 - 260 °C473 - 500 °FInjection Molding
 245 - 260 °C473 - 500 °FCompounding Extrusion
Mold Temperature 50.0 - 75.0 °C122 - 167 °F
Drying Temperature 110 - 120 °C230 - 248 °FCompounding Extrusion
 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 4.00 - 6.00 hour4.00 - 6.00 hourCompounding Extrusion
 8.00 hour8.00 hourCumulative; Compounding Extrusion
 12.0 hour12.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00130 - 0.00250 cm0.000512 - 0.000984 in
Screw Speed 50 - 100 rpm50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80580 / 288527

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.