MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SCG Chemicals M3804RW Linear-low density polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: SCG LLDPE M3804RW is a linear-low density polyethylene (LLDPE) for rotational molding applications. M3804RW is a natural color PE resin available in a pellet and powder form, whereas M10 is the color compound version. These grades are suitable for rotational molding of storage tanks and general purpose applications.

Applications: Water storage tanks, Small to medium tanks (<5,000 L), Material handling containers, Intermediate bulk containers (IBC).

Features: High stiffness. High thermal stability. Good impact strength. High UV protection (UV8) for outdoor use.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D 1505
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength at Break 18.0 MPa2610 psiCrosshead speed 50 mm/min.; ASTM D638
Tensile Strength, Yield 20.0 MPa2900 psiCrosshead speed 50 mm/min.; ASTM D638
Elongation at Break 800 %800 %Crosshead speed 50 mm/min; ASTM D638
Flexural Modulus 0.700 GPa102 ksiASTM D790
Impact 27
@Thickness 5.50 mm,
Temperature -40.0 °C
27
@Thickness 0.217 in,
Temperature -40.0 °F
J/mm ARM Method, rotomolded
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM D2117
Crystallization Temperature 113 °C235 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C149 °FASTM D648
Vicat Softening Point 116 °C241 °FASTM D1525
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746
 
Descriptive Properties
AppearanceColored compound pellet
 Colored compound powder
 Natural pellet
 Natural powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC738 / 277995

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.