Description: Dymalink® 636 is a solid calcium diacrylate for use in applications requiring a slower cure rate than other acrylate coagents. It is recommended for general purpose peroxide curing of thermoplastic elastomers, particularly chlorinated elastomers. The product is useful in molding or extrusion applications. Product Highlights / Performance Properties: - Slower cure without scorch retardant
- Improved dynamic flex properties
- High tensile strength
Suggested Applications: Information provided by Cray Valley |