MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Proto3000 – 3D Engineering Solutions

(Viewing data as-entered. Click here to return)
RESPOL REPSOL PRIMEVA® P33400 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA resin REPSOL PRIMEVA® P33400 is recommended for low viscosity hot melt adhesives applications, when low viscosity and high vinyl acetate content are required. EVA resin REPSOL PRIMEVA® P33400 has been improved for a better stability against thermal degradation. It contains antioxidant and free flowing agent.
Applications: Hot Melt Adhesives – Packaging, Bookbinding, Furniture, Pressure sensitive adhesive coatings
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant; Free Flowing Agent

Features: Antioxidant; Copolymer; Food Contact Acceptable; Good Thermal Stability; Low Viscosity

Uses: Adhesives; Furniture; Packaging

Agency Ratings: EU Food Contact

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.957 g/ccISO 1183
Vinyl Acetate Content 33 %
Melt Flow 400 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55ISO 868
Tensile Strength at Break 290 psiISO 527-2
Elongation at Break 900 %ISO 527-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 142 °F
Ring & Ball Softening Point 172 °FASTM E28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESPOL1347 / 312040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.