MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 201-67W171 Thermoplastic Vulcanizate Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable thermoplastic vulcanizate (PTV) in the thermoplastic elastomer family. This material is formulated for low density foamed profile extrusion applications and has long term salability, low temperature flexibility and hear weldability. This grade of Santoprene TPV is shear dependent and can be processed using specially adapted physical foam extrusion lines. It is polyolefin based and recyclable within the manufacturing stream. Availability: Africa & Middle East, Europe, Asia Pacific, Latin America, North America. RoHS compliant. Color: natural. Forms: Pellets. Processing Method: Foam extrusion.

Information provided by Exxon Mobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
@Time 15.0 sec
ISO 868
Tensile Strength at Break 1000 psiAcross Flow; ASTM D412
Elongation at Break 450 %Across Flow; ASTM D412
100% Modulus 0.406 ksi
@Strain 100 %
Across Flow; ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas EZPrene 9070A TPV
Mitsui Milastomer™ 7030BS Black Vulcanized Thermoplastic Elastomer
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer

PEXA906f / 233597

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.