MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Colorite Polymers Self Frosting™ 8011SF Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, this was accomplished by using cold die techniques that reduced production rates by as much as 20%. This method also generates substantial amounts of scrap or rejected material due to imperfect frosting. Colorite SF compounds permit the user to maintain production rates with a uniform reproducible matte finish. Colorite SF compounds are available in non-toxic grades for the food and medical industries where the need for a low surface friction tubing exists and total transparency is not necessary.

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.235 g/cc1.235 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Tensile Strength, Ultimate 17.6 MPa2550 psi
Elongation at Break 350 %350 %
100% Modulus 8.76 MPa
@Strain 100 %
1270 psi
@Strain 100 %
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -29.0 °C-20.2 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers 6077 Non-Phthalate 77 Series Vinyl Compound
Colorite Polymers 8011G-015 (Extrustion), 8012G-015 (Molding) Radiation Sterilizable Vinyl Compound
Colorite Polymers Elastichem 6011TX-02 Vinyl Compound
Colorite Polymers 9812-15 Radiopaque Vinyl Compound
Colorite Polymers 8077 Non-Phthalate 77 Series Vinyl Compound

PCOL162 / 28881

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.