MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Inov Chem Donspray 504 HFC-245fa Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonSpray504 is spray blend polyols, blowing agent is 245fa instead of HCFC-141B, it reacts with isocyanate to produce foam which has excellent performances, which are as follows,
1) fine and uniformity cells
2) low thermal conductivity
3) perfect flame resistance
4) good low-temperature dimensional stability.
It applies to all kinds of thermal insulation engineering which uses the spray technology, such as cold rooms, pots, large-scale pipelines and construction metope etc.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 - 1.20 g/cc1.12 - 1.20 g/cc
Density >= 0.0350 g/cc>= 0.00126 lb/in³Spray Density; GB 6343
Water Absorption <= 3.0 %<= 3.0 %GB 8810
Viscosity 100 - 200 cP100 - 200 cPDynamic
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 0.150 MPa>= 21.8 psiGB/T8813
Adhesive Bond Strength >= 0.120 MPa>= 17.4 psiGB/T16777
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity <= 0.0240 W/m-K
@Temperature 15.0 °C
<= 0.167 BTU-in/hr-ft²-°F
@Temperature 59.0 °F
GB 3399
 
Processing PropertiesMetricEnglishComments
Gel Time 0.100 - 0.167 min0.100 - 0.167 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AppearancePale yellow to brown viscous liquid
Closed-cell rate=90%GB 10799
Cream time3-5 sec
Dimensional stability=1.0%24h, -20?; GB/T8811
 =1.5%24h, 70?; GB/T8811
FlammabilityClass B2GB 8624
Hydroxyl value200-300 mgKOH/g
Recommended Ratio100 gDonSpray 504 blend polyols
 100-105 gIsocyanate MDI

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM025 / 312554

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.