MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SeBiLOY II (EnviroBrass II), Copper Alloy, UNS C89520, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Casting Yield; Medium – Drossing, Fluidity, Gassing, Shrinkage in Solidification; Low –Effect of Section Size

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing

Typical uses: Plumbing Castings

Applicable Specifications: As Sand Cast – B584; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 54
@Load 500 kg
54
@Load 1100 lb
Tensile Strength 214 MPa31000 psi
Tensile Strength, Yield 145 MPa21000 psi0.5% Ext
Elongation at Break 10 %10 %
Machinability 85 %85 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 - 1006 °C353 - 1842 °F
Solidus 178 °C353 °F
Liquidus 1006 °C1842 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.25 %<= 0.25 %
Bismuth, Bi 1.6 - 2.2 %1.6 - 2.2 %
Copper, Cu 85 - 87 %85 - 87 %
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.090 %<= 0.090 %
Nickel, Ni <= 1.0 %<= 1.0 %
Selenium, Se 0.80 - 1.1 %0.80 - 1.1 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 5.0 - 6.0 %5.0 - 6.0 %
Zinc, Zn 4.0 - 6.0 %4.0 - 6.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC89520x1 / 292577

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.