MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Accelerator 19GB Accelerator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: LORD® Accelerator 19GB is a mix-in curative designed for use with LORD acrylic adhesives. LORD Accelerator 19GB, when mixed with LORD 200, 400 or 500 series acrylic adhesives, creates adhesive systems that will bond a variety of prepared or unprepared metals and plastics. LORD Accelerator 19GB allows precise control of adhesive bondline thickness due to its content of glass beads, 0.01" (0.025 cm) diameter.

Features: provides room temperature cure with all LORD acrylic adhesives. contains no solvent, non-flammable and virtually odorless. resists common environmental conditions when used with LORD acrylic adhesives. improves high temperature resistance of LORD 200, 400 and 500 series acrylic adhesives.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 - 1.576 g/cc0.0537 - 0.05693 lb/in³Red
 1.480 - 1.58 g/cc0.05346 - 0.0571 lb/in³Off-White
 1.552 - 1.64 g/cc0.05606 - 0.0593 lb/in³Grey
Solids Content 99.07 %99.07 %by weight
Brookfield Viscosity 100000 - 400000 cP
@Temperature 25.0 °C
100000 - 400000 cP
@Temperature 77.0 °F
Brookfield Model HAT, T-bar C 5rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month
@Temperature 16.0 - 27.0 °C
9.00 Month
@Temperature 60.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceGrey PasteAccelerator 19GB, Red
 Off-white pasteAccelerator 19GB
 Red PasteAccelerator 19GB, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9106 / 232494

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.