TROGAMID® myCX eCO is a microcrystalline transparent polyamide for the manufacture of parts in the optical industry, like lenses according the injection molding procedure. TROGAMID® myCX eCO is set up with production technology using maximal saving potential for CO2 emission up to 50%. TROGAMID® myCX eCO is supplied as spherical pellets in moisture-proof packaging.Preliminary data sheet. Industrial Sector: Sustainable, Optics, Sports and Lifestyle Sustainability: eCO Processing: Injection molding , Extrusion Optics: Transparent, High gloss, X-ray transparent Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Fatigue resistance Conformity: Food contact Additives: Unfilled Applications: Fiber optic cable, (Sun-) glasses, Hygiene and cosmetics, Lenses, Monofilament Processing: Film extrusion Special Characteristics: Halogen-free, Phosphorus-free, High impact strength, Low viscosity Features: optical UV-protection, Weldable, Low birefringence, Non-corrosive, Dishwasher detergents resistant Regulatory: Food contact 10/2011/EC Color: Natural color Delivery form: Spherical pelletsInformation provided by Evonik. |