MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC LNP™ THERMOCOMP™ Compound LX09404 Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LX09404 compound is based on Polyetheretherketone (PEEK) resin containing 45% carbon fiber. Added features of this grade include: Electrically Conductive, High Modulus

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Moisture Absorption 0.410 %0.410 %23°C/50% RH/24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 280 MPa40600 psi5 mm/min; ASTM D638
Elongation at Break 1.3 %1.3 %5 mm/min; ASTM D638
Tensile Modulus 41.5 GPa6020 ksi5 mm/min; ASTM D638
Flexural Strength 424 MPa61500 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 29.65 GPa4300 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 93.0 J68.6 ft-lbASTM D256
Izod Impact, Unnotched 8.28 J/cm15.5 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 332 °C
@Thickness 3.20 mm
630 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 380 - 400 °C716 - 752 °F
Zone 3 380 - 400 °C716 - 752 °F
Mold Temperature 175 - 190 °C347 - 374 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 60 - 100 rpm60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81701 / 289648

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.