MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CeramTec Rubalit® 702 Alumina, 85%
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical applications have shown that Rubalit® 702 is capable of diffusing as much heat as the cap and film. Its extreme hardness necessitates laser trimming of the film material.

Key Words: Al2O3, aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.55 g/cc0.128 lb/in³DIN EN 623-2 / ASTM-C373 / ASTM-C20
Water Absorption 0.00 %0.00 %DIN EN 623-2 / ASTM-C373
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 45 N 7373ASTM-E18
Vickers Microhardness 7373HV 0.5; DINV ENV 843-4
Flexural Strength 390 MPa56600 psi20 x 40 mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1.00e+8 ohm-cm
@Temperature 600 °C
1.00e+8 ohm-cm
@Temperature 1110 °F
ASTM-D1829
 1.00e+10 ohm-cm
@Temperature 400 °C
1.00e+10 ohm-cm
@Temperature 752 °F
ASTM-D1829
 1.00e+12 ohm-cm
@Temperature 200 °C
1.00e+12 ohm-cm
@Temperature 392 °F
ASTM-D257
Dielectric Constant 8.0
@Frequency 1e+6 Hz
8.0
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-C150
Dielectric Strength >= 10.0 kV/mm>= 254 kV/inASTM-D150
Dielectric Loss Index 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
IEC 672-1 / ASTM-D149,150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.50 µm/m-°C
@Temperature 20.0 - 100 °C
2.50 µin/in-°F
@Temperature 68.0 - 212 °F
ASTM-C372
 6.20 µm/m-°C
@Temperature 20.0 - 300 °C
3.44 µin/in-°F
@Temperature 68.0 - 572 °F
ASTM-C372
 7.00 µm/m-°C
@Temperature 20.0 - 600 °C
3.89 µin/in-°F
@Temperature 68.0 - 1110 °F
ASTM-C372
 7.80 µm/m-°C
@Temperature 20.0 - 1000 °C
4.33 µin/in-°F
@Temperature 68.0 - 1830 °F
ASTM-C372
Thermal Conductivity 16.0 W/m-K111 BTU-in/hr-ft²-°FDIN EN 821-2 / ASTM-C408
Maximum Service Temperature, Air 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 85 %85 %
 
Descriptive Properties
ColorWhite
Ra = Arithmetic Mean Roughness Value (µm)0.2-0.3
Te Value (°C)850

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
CeramTec V 679 Alumina, 99.7%
Alumina, alpha Al2O3, 99.5%
Alumina, alpha Al2O3, 96%
CeramTec B 601 Alumina, 98.5%

CCERA929 / 107529

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.