MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vibrantz Technologies EG 2760 Thick Film Glass
Categories: Ceramic; Glass

Material Notes: Glass Type: Pb-B-Zn
Typical Powder Form: MVG, VEG
Typical Application: General

Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conductors, end terminations, over glazes, and dielectrics.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.55 g/cc
Particle Size 5.0 µm50% of particles, (MVG Powder)
 10 µm50% of particles, (VEG Powder)
 <= 25 µmMVG Powder
 <= 74 µmVEG Powder
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.9 µm/m-°Cat Set Pt.
 11.35 µm/m-°C
@Temperature 260 °C
Softening Point 350 °C
Annealing Point 325 °C
Transformation Temperature 315 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 °CTypical Firing Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass
Corning Gorilla® Glass 5 Display Glass
Vibrantz Technologies EG 2705 Glaze and Sealant Glass
Vibrantz Technologies EG 2738 Dental Glass
Corning 1724 Aluminosilicate Crushed/Powdered Glass

CFERR65 / 879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.