MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALFATER® XL A60E 2GP0000 PP/EPDM
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Base Polymer: Thermoplastic Vulcanisate PP/EPDM-Elastomer

Special Features: Good weathering resistance, resistant to alkalis, resistant to ozone, resistant to hot air, hydrolysis resistant

Market Segment: Automotive, Building and Construction, Electrical and Electronic

Application Area: Extruded parts, blow molded parts

Typical Applications: Profiles, seals, conduit, tubes, cable guides, cable jacketing, bellows

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60
@Time 15.0 sec
60
@Time 0.00417 hour
ISO 868
Tensile Strength 5.40 MPa783 psitype 2; ISO 37
Tensile Stress at Strain 2.50 MPa
@Strain 100 %
363 psi
@Strain 100 %
type 2; ISO 37
Elongation at Break 350 %350 %type 2; ISO 37
Tear Strength 22.0 kN/m126 plimethod Ba; ISO 34-1
Compression Set  22 %
@Temperature 22.0 °C,
Time 259000 sec
22 %
@Temperature 71.6 °F,
Time 72.0 hour
25%, Type A; ISO 815
 37 %
@Temperature 100 °C,
Time 79200 sec
37 %
@Temperature 212 °F,
Time 22.0 hour
25%, Type A; ISO 815
 38 %
@Temperature 70.0 °C,
Time 79200 sec
38 %
@Temperature 158 °F,
Time 22.0 hour
25%, Type A; ISO 815
 55 %
@Temperature 125 °C,
Time 259000 sec
55 %
@Temperature 257 °F,
Time 72.0 hour
25%, Type A; ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 240 °C392 - 464 °FExtrusion
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
158 - 176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerThermoplastic Vulcanizate PP/EPDM-Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALFATER® XL A30I 4GP0000 PP/EPDM

PALBIS8214 / 242273

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.