MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kaltun CERATUN FELDSPAR S.SAB.673 for Ceramic Production
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: CERATUN feldspar is used in ceramic, granite, technical porcelain, vitrified, frit, glaze, engobe, tableware productions. All CERATUN products are produced in mines belonging to Kaltun Madencilik A.S. and located in the Çine-Milas region.

Information provided by KALTUN MINING

Key Words: Product Code: KSS.14.B.0005
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³
Moisture Absorption 3.00 %3.00 %Summer Humidity
 5.00 %5.00 %Winter Humidity
Loss On Ignition 2.5 %2.5 %
Particle Size >= 500 µm>= 500 µm45% Screening (wet/dry)
 <= 500 µm<= 500 µm55% Screening (wet/dry)
 >= 5000 µm>= 5000 µm5% Screening (wet/dry)
 >= 10000 µm>= 10000 µm0% Screening (wet/dry)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.06.0
 
Component Elements PropertiesMetricEnglishComments
Al2O3 17.15 %17.15 %
CaO 0.87 %0.87 %
Fe2O3 0.17 %0.17 %
K2O 0.38 %0.38 %
MgO 2.25 %2.25 %
Na2O 9.2 %9.2 %
P2O5 0.31 %0.31 %
SiO2 66.85 %66.85 %
TiO2 0.32 %0.32 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKALT808 / 318106

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.