MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-NA-2200 Transparent Nucleating Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Polypropylene(2401) : 98.5% GY-NA-2000 series : 1.5%

Intro:

  • GY-NA-2200 series are new class of nucleating agents capable of inducing crystal growth in the polymer . This series product act as a nucleating agent by creating a large number of small size crystalline structure during the cooling of the polypropylene melt
  • GY-NA-2200 series improves mechanical properties, clarity of polypropylene, heat resistance, size stability and surface gloss.
  • GY-NA-2200 series product make injection molders achieve better production speeds and broaden the molding condition.
Features:
  • Enhance the mechanical strength
  • Improve crystal growth in the polymer
  • Improve the clarity of goods
  • Provide long-term heat stability
  • Enhance the stability of melting for polymers.
  • By using GY-NA-2200 series, it can be anti-aging, antifragile during the processing of organic polymer
Applications:
  • PP (Polypropylene)
  • PET (Polyethylene terephthalate)
  • PBT (Polybutylene terephthalate)
  • PC (Polycarbonate)
  • PMMA (Polymethyl Methacrylate)
  • Polyamide
  • Polyolefin( HDPE , LDPE , EVA , PVC )
  • Others & Elastomer (TPU,TPE.TPV.SBS)

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength <= 37.1 MPa
Impact 4.0[kg/m2], Impact resistance ratio
 
Optical PropertiesOriginal ValueComments
Haze 37 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN343 / 266651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.