MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ed Fagan EFI Alloy 79 Soft Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy

Material Notes: Features extremely high initial & maximum permeability and minimum hysteresis. Composition is equivalent to: Magnifer 7904, HyMu 80, Hipernom, Moly-Permalloy, Permalloy 80.

Key Words: ASTM A753, MIL N-14411C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.316 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85
Tensile Strength, Ultimate 676 MPa
Tensile Strength, Yield 262 MPa
Elongation at Break 40 %in 2"
Modulus of Elasticity 217 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000590 ohm-cm
Magnetic Permeability 230000Typical DC
Magnetic Coercive Force, Hc 0.015 OeTypical DC
Magnetic Saturation Flux Density, Bmax 8700 GaussTypical DC
Curie Temperature 460 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.50 µin/in-°F
@Temperature 25.0 - 450 °C
Thermal Conductivity 240 BTU-in/hr-ft²-°F
Melting Point 1454 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.03 %
Iron, Fe 15 %as Balance
Manganese, Mn <= 0.95 %
Molybdenum, Mo <= 5.0 %
Nickel, Ni 80 %Nominal
Phosphorus, P <= 0.02 %
Silicon, Si <= 0.42 %
Sulfur, S <= 0.008 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ed Fagan EFI Alloy 50 Soft Magnetic Alloy
Alloy Wire International RW 45 Ni-Cu Resistance Wire
Constantan Thermocouple Wire
Cunife® Hard Magnetic Alloy
Eagle Brass 752 Nickel Silver 18%, Hard

NEDFA9979 / 194941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.