MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
JSC SKS-30 ARK (SBR 1500) and SKS-30 ARKPN (SBR-1502) Styrene-butadiene rubber
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: NON-SPECIFIED SYNTHETIC STYRENE-BUTADIENE RUBBERS SKS-30 ARK (SBR-1500) and SKS-30 ARKPN (SBR-1502)

Description: Styrene-butadiene rubbers SKS-30 ARK (SBR-1500) and SKS-30 ARKPN (SBR-1502) are a styrene and butadiene copolymer obtained by cold emulsion polymerization using rosin and fatty acids soaps mix as an emulsifier. It is stabilized by non-staining antioxidant.

Application: for use in various branches of industry.

Appearance: briquettes (bales) or irregularly shaped briquettes (bales)

Color: from white to dark-yellow

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 8.0 %ASTM D5668 (method C)
Mooney Viscosity <= 60
@Temperature 100 °C
ML 1+4; ASTM D 1646 (para.7.2.2.)
Ash <= 1.2 %ASTM D 5667 (part A)
Storage Temperature <= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Content>0.4%Antioxidant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC016 / 317836

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.