MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ THERMOCOMP™ OF008AE PPS - Branched (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP* THERMOCOMP* OF008AE is a compound based on PPS - Branched resin containing 40% Glass Fiber. Added feature of this grade is: Easy Molding.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D 792
Density 1.70 g/cc0.0614 lb/in³ASTM D 792
Moisture Absorption 0.130 %
@Temperature 23.0 °C
0.130 %
@Temperature 73.4 °F
50% RH; ISO 62
 0.210 %
@Time 86400 sec
0.210 %
@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0036 cm/cm
@Time 86400 sec
0.0036 in/in
@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.012 cm/cm
@Time 86400 sec
0.012 in/in
@Time 24.0 hour
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 128 MPa18600 psi5 mm/min; ISO 527
 133 MPa19300 psiType I, 5 mm/min; ASTM D 638
Elongation at Break 0.90 %0.90 %5 mm/min; ISO 527
 0.90 %0.90 %Type I, 5 mm/min; ASTM D 638
Tensile Modulus 16.34 GPa2370 ksi1 mm/min; ISO 527
 17.04 GPa2471 ksi5 mm/min; ASTM D 638
Flexural Strength 197 MPa28600 psiISO 178
 205 MPa29700 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 15.45 GPa2241 ksi2 mm/min; ISO 178
 16.1 GPa2340 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.900 J/cm
@Temperature 23.0 °C
1.69 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.97 J/cm
@Temperature 23.0 °C
5.56 ft-lb/in
@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Total Energy 4.00 J
@Temperature 23.0 °C
2.95 ft-lb
@Temperature 73.4 °F
ASTM D 3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
10.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D 696
CTE, linear, Transverse to Flow 37.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
20.6 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 277 °C531 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 280 °C
@Thickness 3.20 mm
536 °F
@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 366 °C691 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 271 °C
@Thickness 3.20 mm
520 °F
@Thickness 0.126 in
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI47040 / 188125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.