MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® 2075MT High Impact ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: ALLEN® 2075MT is a general purpose ABS that has high impact strength and a good cost to performance ratio to other materials like stainless steel, and other thermoplastics.

ALLEN® 2075MT has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Recreational vehicles
  • Agricultural cab interiors
  • Truck interiors
  • Equipment covers
  • POP Displays
Features:
  • Custom color matching
  • Ease of processing
  • Regrind compatible in future orders
  • Matte gloss finish

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Moisture Absorption 0.270 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 93.0ASTM D785
Tensile Strength, Yield 42.0 MPaASTM D638
Tensile Modulus 1909.8 MPaASTM D638
Flexural Strength 63.4 MPa
@Strain 5.00 %
ASTM D790
Flexural Modulus 1990 MPaASTM D790
Compressive Yield Strength 47.5 MPaASTM D695
Bearing Yield Strength <= 177.2 MPaASTM D953
 20.3 MPa
@Strain 4.00 %
ASTM D953
Shear Strength 39.2 MPaASTM D732
Izod Impact, Notched 165.5 J/m
@Temperature -29.0 °C
ASTM D256
 283.5 J/m
@Temperature 23.0 °C
ASTM D256
Gardner Impact 24.7 J
@Temperature -29.0 °C
Drop Dart Impact, GE; ASTM D5420
 46.1 J
@Temperature 23.0 °C
Drop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 20.4 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 97.7 µm/m-°CASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.2 °Cannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °Cannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS564 / 325304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.